Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Omni Plastics OmniTuff™ CPP GRC10 Copolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | |
Parylene Coating Services N Poly (P-Xylylene) Monomer is para-xylylene. Parylene N has a lower coefficient of friction and therefore is recommended where lubricity is needed. Parylene N exhibits a slight haze at thicknesses over 5 microns.Par.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2000NHL Nylon 6 (Cond) Information provided by Ravago. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Global GP-150 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM-D638 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® ABS/PBT 1500 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 SF76 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (76%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 SF80 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (80%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Plastiblend® PBT/ABS BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Techmer ES Electrablend® PA6 IM A Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Conductive, Impact Modified, Heat Stabilized and LubricatedAppearance: BlackInformation pro.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Chase Plastics CP Pryme® NNA100 (Dry) ABS Polyamide Alloy Features: Good abrasion resistancePleasing surface appearanceGood chemical resistanceHigh impact resistanceHigh rigidityLow shrinkageSolvent resistanceHigh strengthGood thermal stabilityGood toughne.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3001MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D638 |
Clariant Renol CAB1000 Cellulose Acetate Butyrate Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall HH-2000 Rigid PVC, Molding Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent .. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall 3217 Rigid PVC, Extrusion Georgia Gulf 3217 is a powder blend designed for the extrusion of window, door, fence and marine profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall 7777 Rigid PVC, Extrusion Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall 9209 Rigid PVC, Molding Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall Suprel® SVA 9301 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li.. |
|||
Tensile Strength, Yield | 43.4 - 90.3 MPa | 6300 - 13100 psi | Average value: 75.3 MPa Grade Count:22 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM D-638 |
Axiall 2651 Rigid PVC, Molding Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 43.4 MPa | 6300 psi | ASTM 638 |
PlastxWorld CEVIAN® B45M0 PBT/ABS Alloy These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |