PlastiComp Complet® LCF30-PPS Polyphenylene Sulfide, 30% Long Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF30-PPS Polyphenylene Sulfide, 30% Long Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphenylene Sulfide with 30% long carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D-792
Filler Content 30 %
30 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 187 MPa
27100 psi
ASTM D-638
Elongation at Break 0.70 %
0.70 %
ASTM D-638
Tensile Modulus 33.793 GPa
4901.3 ksi
ASTM D-638
Flexural Strength 297 MPa
43100 psi
ASTM D-790
Flexural Modulus 25.517 GPa
3700.9 ksi
ASTM D-790
Izod Impact, Unnotched 4.65 J/cm
8.71 ft-lb/in
ASTM D-4812