Tensile Strength 187 MPa
27100 psi
ASTM D-638
PlastiComp Complet® LCF30-PPS Polyphenylene Sulfide, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphenylene Sulfide with 30% long carbon fiber reinforcementInformation provided by ..