Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 187 MPa | 27100 psi | ASTM D-638 |
PlastiComp Complet® LCF30-PPS Polyphenylene Sulfide, 30% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphenylene Sulfide with 30% long carbon fiber reinforcementInformation provided by .. |