Material Notes:
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 17.55 g/cc
17.55 g/cc
Mechanical Properties Metric English Comments
Tensile Strength 1465 - 1525 MPa
212500 - 221200 psi
Tensile Strength, Yield 1450 - 1510 MPa
210000 - 219000 psi
Elongation at Break 5.0 - 8.0 %
5.0 - 8.0 %
Charpy Impact, Notched 30.0 - 60.0 J/cm²
143 - 286 ft-lb/in²
Component Elements Properties Metric English Comments
Other, total 2.5 - 10 %
2.5 - 10 %
Ni + Fe + Co
Tungsten, W 90 - 97.5 %
90 - 97.5 %
Descriptive Properties Value Comments
Ductility much greater than pure W
Fineness of Grain greater than pure W
Machinability/Workability much greater than pure W