Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1465 - 1525 MPa | 212500 - 221200 psi | |
Plansee DENAL® 917 108 XXX (3) Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |