Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 17.55 g/cc | 17.55 g/cc | |
Plansee DENAL® 917 108 XXX (1) Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |
|||
Specific Gravity | 17.55 g/cc | 17.55 g/cc | |
Plansee DENAL® 917 108 XXX (2) Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |
|||
Specific Gravity | 17.55 g/cc | 17.55 g/cc | |
Plansee DENAL® 917 108 XXX (3) Tungsten-Nickel-Iron-Cobalt Alloy Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee. |