Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics Tecknit
Trade Name SC-Consil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows SC-CONSIL to maintain its physical and electrical properties over an extremely wide temperature range. SC-CONSIL is manufactured in sheets, molded and continuously extruded strips, and in die-cut gasketTypical Applications SC-CONSIL provides excellent voltage handling capabilities for grounding, lower current densities, and is ideal for static discharge and corona applications. Various extruded shapes designed for groove and flange mounting, such as tubes and P-shapes, provide maximum deflection at low to medium closure pressures. SC-CONSIL also provides a good environmental seal under moderate closing forcesInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.28 g/cc
1.22 - 1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 75
60 - 75
ASTM D2240
Tensile Strength >= 4.48 MPa
>= 650 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Tear Strength 8.77 kN/m
50.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity <= 15 ohm-cm
<= 15 ohm-cm
Shielding Effectiveness 56 dB

@Frequency 1.00e+9 Hz
56 dB

@Frequency 1.00e+9 Hz
Plane Wave
72 dB

@Frequency 1.00e+7 Hz
72 dB

@Frequency 1.00e+7 Hz
E-Field
88 dB

@Frequency 1.00e+10 Hz
88 dB

@Frequency 1.00e+10 Hz
Plane Wave
93 dB

@Frequency 100000 Hz
93 dB

@Frequency 100000 Hz
H-Field
Descriptive Properties Value Comments
Binder Silicone
Color Black
Filler Carbon