Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PSM Industries Pacific Sintered Metals Yellow Brass BZ-111-U Powdered Metal

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer PSM Industries
Trade Name Pacific Sintered Metals
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Pacific Sintered Metals Yellow Brass BZ-111-U Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
80-20 leaded brass for structural and hardware components Equivalent MPIF Specification: CZP-2000-11Information Provided by Pacific Sintered Metals, a division of PSM Industries
Physical Properties Metric English Comments
Density 7.60 - 7.80 g/cc
0.275 - 0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 70
70
Tensile Strength, Ultimate 159 MPa
23000 psi
Tensile Strength, Yield 93.1 MPa
13500 psi
Elongation at Break 12 %
12 %
1 in. gauge
Flexural Strength 345 MPa
50000 psi
Transverse Rupture
Charpy Impact, Unnotched 38.0 J
28.0 ft-lb
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000690 ohm-cm
0.00000690 ohm-cm