Polymer Property : Tensile Strength, Yield = 93.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.1 MPa
13500 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Nymax™ MF 1200 A 40 HS Natural Polyamide 66 (Nylon 66)
The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc..
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced
Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Tensile Strength, Yield 93.1 MPa
13500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)  (discontinued **)
Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 93.1 MPa
13500 psi
PSM Industries Pacific Sintered Metals Yellow Brass BZ-111-U Powdered Metal
80-20 leaded brass for structural and hardware components Equivalent MPIF Specification: CZP-2000-11Information Provided by Pacific Sintered Metals, a division of PSM Industries
Tensile Strength, Yield 93.1 MPa
13500 psi
Pacific Sintered Materials BZ-111-U Yellow Brass Powdered Metal
Applications: 80-20 leaded brass for structural and hardware components.Equivalent MPIF Specification: CZP-2000-11All information provided by Pacific Sintered Metals.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced
Acrylonitrile Butadiene Styrene, 25% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Tensile Strength, Yield 93.1 MPa
13500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM)
Information provided by Ravago.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Fiberfil® J-60/40/E8 Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES Luriblend® PA6/6 ML2 HS NAT Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(2%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizerAppear..
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES Luriblend® TPX-PA6/6-01072
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b..
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES HiFill® ABS GF30 IM 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,..
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES HiFill® PBT GF15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES HiFill® PBT GF15 BK001 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: BlackTPCI# 6100111Information provided by TP Composit..
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES HiFill® PBT GF15 RD 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: RedTPCI# 862111Information provided by TP Composites,..
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES HiFill® PBT GF15 WT 096 LE 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: WhiteTPCI# 6862111Information provided by TP Composit..
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES Plastiblend® ABS/PBT GF20
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Asahi Kasei Thermylene® P6-30FG-0687 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Asahi Kasei Thermylene® P7-30FG-0890 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Asahi Kasei Thermylene® P7-30FG-1804 30% Glass Fiber Reinforced, Chemically Coupled
Information provided by Asahi Thermofil
Tensile Strength, Yield 93.1 MPa
13500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
PolyOne Edgetek® AT-20GF/000 FDA Acetal-Copolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 93.1 MPa
13500 psi
Type 1 - Rigids, Break, 0.2 in/min; ASTM D638
PolyOne Edgetek® RA-15GF/000 Polyethersulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Yield 93.1 MPa
13500 psi
ASTM D638
Techmer ES Luriblend® POM CO GF20 TL20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated and CopolymerInformation provided by TP Composites, Inc.