Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 93.1 MPa | 13500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ MF 1200 A 40 HS Natural Polyamide 66 (Nylon 66) The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | |
Pacific Sintered Materials BZ-111-U Yellow Brass Powdered Metal Applications: 80-20 leaded brass for structural and hardware components.Equivalent MPIF Specification: CZP-2000-11All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N2017STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 93.2 MPa @Thickness 3.20 mm |
13500 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON CP6080LP PC+CNT+GF Description: Injection Molding, PC+CNT+GF, Electrostatic Dissipation, Low Surface TribochargeApplication: ATM parts, HDD BracketCAS No. 103598-77-2, 65997-17-3 and 7782-42-5Information provided by L.. |
|||
Tensile Strength, Yield | 93.2 MPa @Thickness 3.20 mm |
13500 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
LG Chemical LUMAX GP5200B PBT+ABS+GF20% Description: Injection Molding Grade, PBT+ABS+GF20%, General PurposeApplication: E&E (Speaker Frame)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 9003-54-7Information provided by LG Chemical |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 93.2 MPa @Thickness 3.20 mm |
13500 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 93.2 MPa | 13500 psi | ASTM D638 |
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF30 IM 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® PBT GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® PBT GF15 BK001 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: BlackTPCI# 6100111Information provided by TP Composit.. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES HiFill® PBT GF15 RD 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: RedTPCI# 862111Information provided by TP Composites,.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Tensile Strength, Yield | 93.2 MPa | 13500 psi | ASTM D638 |
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced |
|||
Tensile Strength, Yield | 93.2 MPa | 13500 psi | ASTM D638 |
Cheng Yu Plastic T889G2 PBT, 20% Glass Fiber |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | ASTM D638 |
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced Information provided by Entec |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
Eurostar Starflam PX08029 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX08029 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 93.0 MPa @Temperature -40.0 °C |
13500 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-30FG-0687 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Asahi Kasei Thermylene® P7-30FG-1804 30% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® RA-15GF/000 Polyethersulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 93.0 MPa | 13500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Tensile Strength, Yield | 93.1 MPa | 13500 psi | ASTM D638 |
Techmer ES Luriblend® POM CO GF20 TL20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated and CopolymerInformation provided by TP Composites, Inc. |