Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Oxford Polymers PC 68 Unfilled Polycarbonate for Injection and Extrusion Molding Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Oxford Polymers PC 912 Unfilled Polycarbonate for Injection and Extrusion Molding Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 9945A PC Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 9945A PC (Europe-Africa-Middle East) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LI1911R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® LSHF PC Clear PolyCarbonate, High Flow, UV Stabilization, Heat StabilizationThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics GELOY CR7501 ASA (Europe-Africa-Middle East) High heat injection moulding grade, blend of ASA/AMSAN. It can be positioned for outside parts in various markets. Various colours. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | |
Ineos Styrenics Polystyrene 145D (NAFTA) A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics pu.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1212FR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1212FRRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC721HFR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Teknor Apex APEX® RE 8003 Polyvinyl Chloride, Rigid Features: High Impact Resistance; Medium Gloss Processing Method: Extrusion Forms: Pellets Additional Information: Performance Characteristics: Yellow Card, Interior, Medium Gloss, Excellent FinishI.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM Data |
Styron CALIBRE™ 891 20 Polycarbonate, General Purpose CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Styron EMERGEâ„¢ 4800-10 Polycarbonate EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 (Asia Pacific) LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder, Impact Modifier. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-10 Polycarbonate CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-20 Polycarbonate CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound R7550 CLR 223V is a general purpose medium/high impact profile extrusion compound developed for ease of process, sparkling clarity and gloss. It has been formulated for UV resistance for interior a.. |