Omni Plastics OmniTech™ HDPE GRC20 Glass Reinforced

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Glass fiber Filled
Manufacturer Omni Plastics
Trade Name OmniTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniTech™ HDPE GRC20 Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and Improved Optical Clarity.Applications:flame retardant storage containers, static dissipative trays, internally lubricated gears and rollers, and NSF compliant pool and filler components. Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.5 MPa
6170 psi
ASTM D638
Flexural Modulus 3.09 GPa
448 ksi
ASTM D790
Izod Impact, Notched 0.956 J/cm
1.79 ft-lb/in
ASTM D256