Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.956 J/cm | 1.79 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ HDPE GRC20 Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |