Omni Plastics OmniLon™ 6/6 PA6/6 GR15 Glass Reinforced Nylon

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Omni Plastics
Trade Name OmniLon™ 6/6
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniLon™ 6/6 PA6/6 GR15 Glass Reinforced Nylon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Flexural Modulus 5.17 GPa
750 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256