Material Notes:
Dry as molded. Injection molding grade. Nylene 454 is the heat stabilized version of 451 recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears, bearings, cams, fasteners, and other load bearing parts. Nylene 454 chemically resists oil and grease. Optimum processing conditions should provide a melt temperature of 460 - 480ºF at the nozzle.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.9 %
1.9 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Yield Strength 102 MPa
14800 psi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Processing Temperature 245 °C
473 °F