Nye Lubricants 813-1 (FG) Synthetic Oil

Category Fluid , Lubricant , PTFE Gellant , Silicone Base
Manufacturer Nye Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 813-1 (FG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 373
373
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 53 cSt
53 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 19 cSt
19 cSt
Base Oil; ASTM D445
Evaporation Loss 0.10 %
0.10 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 316
316
ASTM D217
Penetration P(60), 1/10 mm 333
333
ASTM D217
Oil Separation 4.6 %
4.6 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Recommended
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Recommended
Pour Point -73.0 °C
-99.4 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Sil.(Clrphn)
Gellant Type PTFE