Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Kinematic Viscosity 500 cSt

@Temperature 25.0 °C
500 cSt

@Temperature 77.0 °F
Base Oil; ASTM D445
Evaporation Loss 3.0 %
3.0 %
48 hrs, 250C; ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Recommended
Minimum Service Temperature, Air -18.0 °C
-0.400 °F
Recommended
Pour Point -22.0 °C
-7.60 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Sil.(Phenyl)
Copyright © lookpolymers.com All Rights Reserved