Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -22.0 °C | -7.60 °F | Base Oil; ASTM D97 |
Nye Lubricants 231(SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -22.0 °C | -7.60 °F | Base Oil; ASTM D97 |
Nye Lubricants 437 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -22.0 °C | -7.60 °F | ASTM D97 |
ExxonMobil Enmist EP 150 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Pour Point | -22.0 °C | -7.60 °F | |
ChevronTexaco Cepheus® 150 Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they.. |
|||
Pour Point | -22.0 °C | -7.60 °F | ASTM D97 |
ExxonMobil Enmist EP 150 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Pour Point | -22.0 °C | -7.60 °F | ASTM D97 |
ExxonMobil Enmist EP 220 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Pour Point | -22.0 °C | -7.60 °F | ASTM D97 |
ExxonMobil Enmist EP 220 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |