Nye Lubricants 140B (SO) Synthetic Oil

Category Fluid , Lubricant , Synthetic Ether Base , White Mineral Oil (WMO)
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 140B (SO) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 107
107
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 19 cSt
19 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.1 cSt
4.1 cSt
Base Oil; ASTM D445
Evaporation Loss 1.80 %

@Temperature 121 °C,
Time 605000 sec
1.80 %

@Temperature 250 °F,
Time 168 hour
ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -48.0 °C
-54.4 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type WMO/Ester