Material Notes:
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, material handling, step pads and other applications requiring rigid TPOs. This recyclable product is a tough, high-strength thermoplastic that maintains its properties over a wide temperature range.Information provided by Noble Polymers.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.78 MPa
2579 psi
ASTM D638
Elongation at Break 665.8 %
665.8 %
ASTM D412
Izod Impact, Notched 1.02 J/cm

@Temperature -30.0 °C
1.91 ft-lb/in

@Temperature -22.0 °F
ASTM D256
1.53 J/cm

@Temperature 23.0 °C
2.87 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 15.86 J

@Temperature -30.0 °C
11.70 ft-lb

@Temperature -22.0 °F
ASTM D5420
15.86 J

@Temperature 23.0 °C
11.70 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 800 MPa
116000 psi
ASTM D790
Processing Properties Metric English Comments
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature