Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
Plastcom SLOVALEN PC 71 T 20 PP, 20% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrin..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
Plastcom SLOVALEN PH 63 T 20 PP, 20% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Noble Polymers Regis™ 115090 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
Post shrinkage is 0.31% at 72hr 120°C.; ASTM D955
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
Isotropy
Solvay TECHNYL® A 225F PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
SK Chemicals SKYTHANE® 175A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Plenco 5488 Phenolic, Granular, Injection Molded
PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not ..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Plenco 4311 Phenolic, Granular, Injection Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
Plastcom SLOVALEN PH 73 T 20 PP, 20% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh..
Linear Mold Shrinkage 0.0083 cm/cm
0.0083 in/in
ASTM D955
Mitsui AURUM® PL450C Polyimide  (discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..