Nitriflex Nitrilatex L-550 Carboxylated Acrylonitrile Butadiene Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Nitriflex
Trade Name Nitrilatex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex Nitrilatex L-550 Carboxylated Acrylonitrile Butadiene Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesives manufacture, fibers agglomeration, supported gloves manufacture, impregnation of non-woven, etc. Information provided by Dax Resinas
Physical Properties Metric English Comments
Solids Content 38 - 42 %
38 - 42 %
Method L-001/P-065; ASTM D1417
pH 7.5 - 8.0
7.5 - 8.0
25°C, Method L-003; ASTM D1417
Brookfield Viscosity 10 - 25 cP
10 - 25 cP
(spindle=1, 20 rpm); ASTM D1417
Mooney Viscosity 60 - 75
60 - 75
Method L-020; ASTM D1646
Surface Tension 30 - 45 dynes/cm
30 - 45 dynes/cm
Method L-005/L-040; ASTM D1417
Descriptive Properties Value Comments
Bound Acrylonitrile Content (%) 27 - 31
ASTM D3533
Coagulum Content % 0-0.1
ASTM D1417; Method L-004