Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 10 - 25 cP | 10 - 25 cP | (spindle=1, 20 rpm); ASTM D1417 |
Nitriflex Nitrilatex L-550 Carboxylated Acrylonitrile Butadiene Latex NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive.. |
|||
Brookfield Viscosity | 10 - 25 cP | 10 - 25 cP | (spindle=1, 20 rpm); ASTM D1417 |
Nitriflex Nitrilatex L-550c Carboxylated Acrylonitrile Butadiene Latex NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive.. |