Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 30 - 45 dynes/cm | 30 - 45 dynes/cm | Method L-005/L-040; ASTM D1417 |
Nitriflex Nitrilatex L-550 Carboxylated Acrylonitrile Butadiene Latex NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive.. |
|||
Surface Tension | 30 - 45 dynes/cm | 30 - 45 dynes/cm | Method L-005/L-040; ASTM D1417 |
Nitriflex Nitrilatex L-550c Carboxylated Acrylonitrile Butadiene Latex NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive.. |
|||
Surface Tension | 35 - 45 dynes/cm | 35 - 45 dynes/cm | Method L-005/L-040; ASTM D1417 |
Nitriflex Nitrilatex NTL-350 Styrene Butadiene Latex NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid. Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesive.. |
|||
Surface Tension | 35 - 45 dynes/cm | 35 - 45 dynes/cm | Ring Type; LSY-QB-ID005 |
LG Chemical Lutex 760 SBR Latex Description: Binding Force, Print gloss, High Shear Rheology, Post Treatment Properties, Coater RunnabilityApplication: Art Paper, Paperboard-Single, Top-Film, Blade Coater, Adhesive coated paper an.. |