Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 165 GPa | 23900 ksi | ASTM E855-90, Test Method B |
NiCoForm NiColoy® E Electroformed Nickel-Cobalt NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi.. |