Network Polymers Softflex® 7200

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers Softflex® 7200.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.886 g/cc
0.886 g/cc
ASTM D792
Melt Flow 0.50 g/10 min

@Load 1.00 kg,
Temperature 235 °C
0.50 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
1.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
2.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 77
67 - 77
Instantaneous; ASTM D2240
Tensile Strength, Yield 2.34 MPa
340 psi
chs 20 in/min; ASTM D412
Elongation at Break 160 %
160 %
ASTM D412
Flexural Modulus 0.00889 GPa
1.29 ksi