Physical Properties Metric English Comments
Melt Flow 1.1 g/10 min

@Load 1.00 kg,
Temperature 235 °C
1.1 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
Network Polymers Softflex® 5000
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Melt Flow 1.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers Softflex® 7200
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Melt Flow 1.1 g/10 min

@Load 10.0 kg,
Temperature 190 °C
1.1 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Melt Flow 1.1 g/10 min

@Load 5.00 kg
1.1 g/10 min

@Load 11.0 lb
ISO 1133
Total Lacqtene® 2004 TN 52 HDPE pipe  (discontinued **)
LACQTENE® 2004 TN 52 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2004 TN 52 is best processed between 190 and 230°C.Informa..
Melt Flow 1.1 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.1 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene
BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su..
Melt Flow 1.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Test
Styrolution Luran® S 778 T ASA
Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Melt Flow 1.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers ABS 3501 Black 1302 Injection Molding Grade
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 1.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3501 GF-10
Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc.
Melt Flow 1.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA T-105
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc.
Melt Flow 1.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA T-110
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc.
Melt Flow 1.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA T-115
Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc.
Melt Flow 1.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ASA TW-20
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.