Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers NPS 80-1410 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPS 80-1410 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Injection Molding Grade, Medium Impact, High Melt FlowInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 59
59
ASTM D785
Tensile Strength at Break 26.2 MPa
3800 psi
chs 2 in/min; ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
chs 2 in/min; ASTM D638
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
Annealed; ASTM D648
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Copyright © lookpolymers.com All Rights Reserved