Nabaltec NH 20 Aluminum Hydroxide

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Nabaltec GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec NH 20 Aluminum Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in the production of glass and ceramic productsaluminum fluoride, cryolite and other aluminum saltsfrits and pigmentsmolecular sievescatalystsrefractory productspigments
Physical Properties Metric English Comments
Bulk Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Density 2.40 g/cc
0.0867 lb/in³
Moisture Absorption at Equilibrium 0.10 %
0.10 %
20 - 105 °C
Loss On Ignition 34.6 %

@Temperature 105 - 1000 °C
34.6 %

@Temperature 221 - 1830 °F
Component Elements Properties Metric English Comments
Al2O3 >= 65 %
>= 65 %
Fe2O3 0.020 %
0.020 %
Na2O 0.20 %
0.20 %
SiO2 0.020 %
0.020 %
Descriptive Properties Value Comments
Crystal Structure Gibbsite