Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nabaltec APYRAL® 60CD Al(OH)3

Category Ceramic , Oxide , Aluminum Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Nabaltec GmbH
Trade Name APYRAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec APYRAL® 60CD Al(OH)3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decomposition APYRAL ® does not generate toxic or corrosive gases. In addition, there is a distinct reduction in smoke density. APYRAL ® is effective in the crucial phase of the burning process before the outbreak of a fully developed fire.APYRAL ® can be used as a flame retardant filler in ThermosetsElastomersThermoplasticsCable CompoundsTechnical Rubber CompoundsPressed and cast Plastic PartsThermal Insulation FoamsGlass-fiber reinforced plasticsInformation provided by Nabaltec.
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
Density 2.40 g/cc
0.0867 lb/in³
Brightness 98 %

@Wavelength 457 nm
98 %

@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 28 %
28 %
(ml/100 g)
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Loss On Ignition 34.6 %
34.6 %
Particle Size 1.0 µm
1.0 µm
Median; Laser Diffraction
Specific Surface Area 6.0 m²/g
6.0 m²/g
BET
Mechanical Properties Metric English Comments
Hardness, Mohs 3
3
Optical Properties Metric English Comments
Refractive Index 1.58
1.58
Electrical Properties Metric English Comments
Electrical Resistivity 17000 ohm-cm
17000 ohm-cm
Descriptive Properties Value Comments
Aluminum Hydroxide (%) 99.5
Mechanical Properties as Additive Elongation at break: 180 %
Tensile Strength: 16 MPa
HFFR-EVA cable compound
Sieve Analysis 0.1%
> 45 µm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved