Material Notes:
Ash is 15%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.985 g/cc
0.07171 lb/in³
ASTM D792
Melt Flow 7.9 g/10 min
7.9 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
10 sec; ASTM D-2240
Elongation at Break 379 %
379 %
ASTM D412
Flexural Modulus 0.113 GPa
16.4 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 62.9 kN/m
359 pli
ASTM D624