Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.9 g/10 min | 7.9 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 9002 GREY/BROWN Ash is 15%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 7.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melt Flow | 7.9 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.9 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
Melt Flow | 7.9 g/10 min | 7.9 g/10 min | |
LyondellBasell Alathon® M6061 High Density Polyethylene, Injection Molding Grade This product is from the former Equistar product line. |
|||
Melt Flow | 7.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |
|||
Melt Flow | 7.9 g/10 min | 7.9 g/10 min | ISO 1133 |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Melt Flow | 7.9 g/10 min @Load 2.16 kg, Temperature 235 °C |
7.9 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact str.. |
|||
Melt Flow | 7.9 g/10 min @Load 2.16 kg, Temperature 235 °C |
7.9 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact str.. |