Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® RP 6568 C Natural TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® RP 6568 C Natural TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ASTM 792
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 230 °C
26 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
10 seconds; ASTM D2240
Tensile Strength, Yield 3.79 MPa
550 psi
Elastic; ASTM D412
Elongation at Break 760 %
760 %
Elastic; ASTM D412
Tear Strength 22.8 kN/m
130 pli
ASTM D624
Thermal Properties Metric English Comments
Flame Spread 15 mm/min
0.60 in/min
FM VSS-302
Users viewing this material also viewed the following: