Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.08 GPa | 157 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers SEQUEL® 1485 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1485 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, improved scratch and mar .. |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | ASTM D790 |
Braskem BS 002J HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles up to 60 liters with high ESCR; bottles for surface-active agents. Information provided by Braskem |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | ASTM D790 |
Flint Hills 44S2A Polypropylene Impact Copolymer Features: Phosphorus free additive package for silicon coated applications. Product does not contain animal derived components.Applications: Extrusion: blown and cast filmInformation Provided by Fl.. |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | ASTM D790 |
Greene Tweed ARâ„¢ 1 Abrasive-Resistant Thermoplastic Sand and other abrasives are often a challenge for pump users in the power industry. Clearances on line shaft bearings and bowl wear rings open up, increasing pump vibrations and reducing pump effi.. |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju.. |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 3342M Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, GOOD FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING, INJECTION STRETCH BLOW MOLDING (ISBM) FOR FOOD CONTAINERS, BOTTLES, HOUSEWARES, CRATES |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 3342R Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, HIGH FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING FOR FOOD CONTAINERS, HOUSEWARES, CRATES |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | ASTM D790 |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | ASTM D790 |
Multibase Multi-Flamâ„¢ 0206 PP Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsUses:TubingWire JacketingFurnitureInformation provided by Multibase |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H5211PBL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE80 pipe, non pressure pipesCertification: Certified by LNEI.. |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | 1% secant, 0.05 in/min.; ASTM D790A |
ExxonMobil PP7032E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection-molding, extrusion and thermoforming applications.Availability: North America Features:Good Colorabilit.. |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | |
Dow DOWLEX™ IP-10 High Density Polyethylene Next Generation DOWLEX® IP-10 resin is a high density polyethylene resin specifically designed for reusable case applications including, poultry, fast food, automotive, retail, fresh produce, bever.. |
|||
Flexural Modulus | 1.08 GPa | 157 ksi | |
Dow HDPE 10462N High Density Polyethylene DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability.. |