Monmouth Rubber & Plastics Durafoamâ„¢ P191HD EPDM

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Monmouth Rubber & Plastics
Trade Name Durafoam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Monmouth Rubber & Plastics Durafoamâ„¢ P191HD EPDM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inch thick sheets. These test pieces were exposed for 120 hours to a cycle consisting of: 1. Light at 70°C for 8 hours 2. Dark at 50° C for 4 hours 3. Condensation Cooling for 15 minutesInformation provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.160 g/cc
0.00579 lb/in³
Linear Mold Shrinkage <= 0.017 cm/cm
<= 0.017 in/in
Note 1
Mechanical Properties Metric English Comments
Hardness, Shore OO 30 - 50
30 - 50
Tensile Strength 0.345 MPa
50.0 psi
Elongation at Break >= 150 %
>= 150 %
Compressive Strength 0.0138 - 0.0345 MPa
2.00 - 5.00 psi
0.25
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -67.8 °C
-90.0 °F
Minimum Service Temperature, Air 135 °C
275 °F
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved