Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 5-7 days |
Momentive Performance Materials 1200® Construction Sealant One-part, premium glazing sealant for structural as well as general purpose glazing. Cure Method: Acetoxy. Tack-free time |
|||
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 5-7 days |
Momentive Performance Materials Sanitary 1700â„¢ Construction Sealant One-part, mildew-resistant sealant for ceramic tile, showers, tubs, and plumbing fixtures. Cure Method: Acetoxy. Tack-free time |
|||
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 10-14 days |
Momentive Performance Materials Silpruf® Construction Sealant One-part, for weatherseals, structural glazing, and general purpose sealing. Cure Method: Alkoxy (Neutral). Tack-free time 5 to 10 hr.; Peel Strength 55 lb/in.; Sag/slump 0.1 in.Data provided by the.. |
|||
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 3-5 days |
Momentive Performance Materials Ultraglaze® 4000 Construction Sealant High strength, one-part structural glazing/weathersealing system. Cure Method: Alkoxy (Neutral). Tack-free time 2 to 5 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Sili.. |
|||
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 10-14 days |
Momentive Performance Materials Ultraglaze® SSG 4000AC Construction Sealant High strength, one-part, accelerated-cure structural glazing/weathersealing system.Cure Method: Alkoxy (Neutral). Tack-free time 1 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silico.. |
|||
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 2-4 days |
Momentive Performance Materials UltraPruf® SCS 2300 Construction Sealant One-part, for concrete, masonry, and stone. Matte finish. Cure Method: Alkoxy (Neutral); Tack-free time 5 to 10 hr. Peel Strength 55 lb/in. Sag/slump 0.1 in.Data provided by the manufacturer, GE.. |
|||
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 5-7 days |
Momentive Performance Materials Silglaze® II Construction Sealant One-part, for channel, stop, and butt glazing. Primerless adhesion properties. Cure Method: Methoxy (Neutral). Tack-free time 0.5 hr. Peel Strength 30 lb/in.; Sag/slump 0.1 in.Data provided by .. |
|||
Processing Temperature | 27.0 °C | 80.6 °F | Cure time to 0.38 in. is 5-7 days |
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant High strength, two-part structural glazing system. Cure Method: Condensation. Tack-free time 3 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of .. |