Michelman® Michem® Wood Coating 75 Anionic paraffin blend emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Wood Coating
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Wood Coating 75 Anionic paraffin blend emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic paraffin blend emulsionUsage: Michem® Wood Coating 75 provides excellent water resistance for topical wood coatings. This product works to prevent the swelling of wood in the presence of water, as well as providing great water bead with lower VOC.Michem® Wood Coating products are typically used for: Deck stains and sealants for water beading, water repellence and swell resistance; Building materials for water beading, water repellence, water resistance and slip resistance; and Interior furniture and flooring for water resistanceInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.930 - 0.950 g/cc
0.930 - 0.950 g/cc
Volatiles 69 - 71 %
69 - 71 %
pH >= 6.0
>= 6.0
Recommended pH of system
8.3 - 10.3
8.3 - 10.3
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance White, low viscosity liquid
Emulsifier Charge Anionic
Solids Type Proprietary