Michelman® Michem® Emulsion 18325 Nonionic polyethylene wax emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 18325 Nonionic polyethylene wax emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic polyethylene wax emulsionUsage: Michem® Emulsion 18325 as an additive provides excellent water and chemical resistance in film coatings.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamFood Contact Information when manufactured in the USA:FDA:175.105: Components of adhesives.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 74.5 - 75.5 %
74.5 - 75.5 %
pH <= 7.0
<= 7.0
Recommended pH of system
9.0 - 10
9.0 - 10
Brookfield Viscosity 5.0 - 30 cP
5.0 - 30 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance Yellow, translucent liquid
Emulsifier Charge Nonionic
Solids Type Polyethylene