Meehanite CC Corrosion Resisting Cast Iron

Category Metal , Ferrous Metal , Cast Iron
Manufacturer Meehanite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meehanite CC Corrosion Resisting Cast Iron.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type CC is a general utility material providing good corrosive resistance. It can be used for slightly acid solutions, alkali solutions at temperatures up to 150 °F and concentrated sulfuric acid at temperatures up to 250 °F.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Mechanical Properties Metric English Comments
Hardness, Brinell 200
200
Tensile Strength, Ultimate 276 MPa
40000 psi