Material Notes:
Brand 837 features: Good spalling characteristics.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are available with a smooth or a unique textured surface that permits pinpoint contact with the load. Sticking can be eliminated as well as providing a surface that breathes, allowing gasses from the ceramic to escape.Applications include firing ceramic capacitors, SOFCs, PZTs, hard and soft ferrites, co-fired substrates and powdered metals. REPTON is available in a wide range of compositions that include a range of alumina, mullite/alumina, zirconia, cordierite, magnesia, and aluminum titanate.
Physical Properties Metric English Comments
Bulk Density 4.20 g/cc
0.152 lb/in³
Density 5.75 g/cc
0.208 lb/in³
calculated from bulk density after subtracting pore volume
Porosity 27 %
27 %
Mechanical Properties Metric English Comments
Flexural Strength >= 18.0 MPa
>= 2610 psi
Thermal Properties Metric English Comments
CTE, linear 8.00 µm/m-°C

@Temperature 300 °C
4.44 µin/in-°F

@Temperature 572 °F
8.00 µm/m-°C

@Temperature 900 °C
4.44 µin/in-°F

@Temperature 1650 °F
Component Elements Properties Metric English Comments
CaO 4.4 %
4.4 %
ZrO2 95.6 %
95.6 %
Descriptive Properties Value Comments
Spall Resist 500°C