Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.75 g/cc | 0.208 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 837 Zirconia + 4.4 mol% Calcia Brand 837 features: Good spalling characteristics.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, ev.. |
|||
Density | 5.75 g/cc | 0.208 lb/in³ | |
MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
Density | 5.75 g/cc | 0.208 lb/in³ | |
CoorsTek StatSafe™ ZDC Static Dissipative Zirconia Specialized StatSafe™ ESD-safe zirconia combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffne.. |