Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 1.50 - 1.80 µm/m-°C | 0.833 - 1.00 µin/in-°F | |
MarkeTech H-2 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |
|||
CTE, linear | 1.50 - 1.80 µm/m-°C | 0.833 - 1.00 µin/in-°F | |
MarkeTech H-3 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |
|||
CTE, linear | 1.50 - 1.80 µm/m-°C | 0.833 - 1.00 µin/in-°F | |
MarkeTech H-4 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |