Mallard Creek Polymers ROVENE® 6105 SBR Latex

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 6105 SBR Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 6105 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion. Its relative low molecular weight and styrene content (45%) permits the formulation of pressure sensitive adhesives with a minimum amount of tackifiers. It was designed to give excellent performance and compatibility with a wide variety of dispersed tackifiers.APPLICATIONS: ROVENE® 6105 is recommended for pressure sensitive permanent label adhesives such as General Purpose, EDP, and Primary Paper Label applications where high tack with no wing-up in required.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 49.5 - 52 %
49.5 - 52 %
Particle Size 0.17 µm
0.17 µm
pH 8.3 - 9.0
8.3 - 9.0
Brookfield Viscosity 90 - 300 cP
90 - 300 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -31.0 °C
-23.8 °F
Chemical Properties Metric English Comments
Styrene Content 45 %
45 %
Descriptive Properties Value Comments
Emulsifiers Anionic