Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 4076 SBR Latex ROVENE® 4076 is a medium firm carboxylated styrene - butadiene emulsion designed for use in formulating high performance architectural coatings including flat wall paints and primer-sealers. When.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 4106 SBR Latex ROVENE® 4106 is a carboxylated styrene-butadiene emulsion that has a very stiff or "boardy" hand. This binder is recommended as a modifier for other SBR non-woven binders to increase strength and.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers Rovene® 4119 Styrene-Butadiene Emulsion Rovene® 4119 imparts a good wet/dry tensile strength, and has good adhesion to a wide variety of surfaces. As such, it makes an excellent base latex for paper and paperboard barrier coating appli.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 4220 SBR Emulsion ROVENE® 4220 is a new developmental polymer specifically designed to be used flooring adhesives as well as an extender for chloroprene and natural latex in contact adhesives and other cohesive an.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 4848 SBR Emulsion ROVENE® 4848 is a new developmental polymer specifically designed to be used in two part spray adhesives for open or closed cell foams and other contact and cold seal applications. Fast breaking .. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers Rovene® 5051 Styrene-Butadiene Emulsion ROVENE® 5051 is a medium-firm, self cross-linking, carboxylated styrene-butadiene latex emulsion. Its styrene content permits the use in formulating carpet and flooring mastics. This versatile po.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 5550 SBR Latex ROVENE® 5550 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This Self-crosslinking binder imparts excellent water and solvent r.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 6105 SBR Latex ROVENE® 6105 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion. Its relative low molecular weight and styrene content (45%) permits the formulation of pressure sensitive adhesi.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 6130 SBR Latex ROVENE® 6130 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of masking and carton sealing tape adhesives. It exhibits excellent compati.. |
|||
Particle Size | 0.17 µm | 0.17 µm | |
Mallard Creek Polymers ROVENE® 9423 SBR Latex ROVENE® 9423 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight and styren.. |