Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -31.0 °C | -23.8 °F | Internal Method |
Polimeri Europa Europrene® BR HV80 Butadiene Rubber Europrene® BR HV80 is a solution polymerized high vinyl butadiene polymer produced by continuous process using an alkyl lithium catalyst. A non-staining antioxidant is added during the production .. |
|||
Glass Transition Temp, Tg | -31.0 °C | -23.8 °F | Internal Method |
Polimeri Europa Europrene® SOL R 72612 Styrene - Butadiene Copolymer Europrene® SOL R 72612 is a solution polymerized, oil extended styrene-butadiene random copolymer. The polymer is extended with a MES oil and contains a non-staining antioxidant. It is produced .. |
|||
Glass Transition Temp, Tg | -31.0 °C | -23.8 °F | |
Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -31.0 °C | -23.8 °F | |
Mallard Creek Polymers ROVENE® 6105 SBR Latex ROVENE® 6105 is a very soft carboxylated styrene - butadiene (SBR) latex emulsion. Its relative low molecular weight and styrene content (45%) permits the formulation of pressure sensitive adhesi.. |
|||
Glass Transition Temp, Tg | -31.0 °C | -23.8 °F | |
LG Chemical LC100 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex.. |
|||
Glass Transition Temp, Tg | -31.0 °C | -23.8 °F | |
Zeon Chemicals Nipol® 1472X Nitrile Powder and Crumb Elastomer Nipol 1472X is a copolymer of butadiene and acrylonitrile of medium-high acrylonitrile contnet modified to contain carboxyl groups. It contains sufficient antioxidant for normal storage conditions. .. |
|||
Glass Transition Temp, Tg | -31.0 °C | -23.8 °F | DSC |
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv.. |
|||
Glass Transition Temp, Tg | -31.0 - -18.0 °C | -23.8 - -0.400 °F | |
Zeon Chemicals Nipol® 1472HV Nitrile Powder and Crumb Elastomer Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is .. |