MV Labs NI1010 (NH4)2Ni(SO4)2·6H2O Ammonium nickel(II) sulfate hexahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NI1010 (NH4)2Ni(SO4)2·6H2O Ammonium nickel(II) sulfate hexahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 394.7 g/mol
394.7 g/mol
Descriptive Properties Value Comments
Assay 15% Ni
CAS Number 7785-20-8
Form Green crystals
Purity 99.999%
Typical Impurities Fe, Mg = 1 ppm