Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled , Nylon 66, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 0.70 %

@Time 86400 sec
0.70 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 86.2 MPa
12500 psi
ASTM D638
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ASTM D638
Flexural Strength 130 MPa
18800 psi
ASTM D790
Flexural Modulus 4.15 GPa
602 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 55.8 µm/m-°C
31.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 227 °C
440 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Strength 18.9 kV/mm
480 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: