Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 589.06 g/mol
589.06 g/mol
Descriptive Properties Value Comments
CAS Number 58176-69-5
Form Pale yellow powder
Purity 99.999%
Typical Impurities Rare Earths < 10 ND; Ca< 5; Si = 2 ppm