Material Notes:
AntistaticImpact copolymerHigh flowGood impact resistanceNucleatedGood stiffnessApplications: FurnitureHousehold goodsOutdoor furnishingsToys
Physical Properties Metric English Comments
Density 0.901 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Characteristics Antistatic, Nucleating agent
Forms Pellets
Processing Methods Injection molding